Awarded as the best online publication by CIDC
WORKABILITY
Slump test is used to determine the workability of fresh concrete. Slump test as per IS: 1199 – 1959 is followed.The apparatus used for doing slump test are Slump cone and Tamping rod.
Procedure to determine workability of fresh concrete by slump test.
i) The internal surface of the mould is thoroughly cleaned and applied with a light coat of oil.
ii) The mould is placed on a smooth, horizontal, rigid and nonabsorbent surface.
iii) The mould is then filled in four layers with freshly mixed concrete, each approximately to one-fourth of the height of the mould.
iv) Each layer is tamped 25 times by the rounded end of the tamping rod (strokes are distributed evenly over the cross section).
v) After the top layer is rodded, the concrete is struck off the level with a trowel.
vi) The mould is removed from the concrete immediately by raising it slowly in the vertical direction.
vii) The difference in level between the height of the mould and that of the highest point of the subsided concrete is measured.
viii) This difference in height in mm is the slump of the concrete.
Reporting of Results
The slump measured should be recorded in mm of subsidence of the specimen during the test. Any slump specimen, which collapses or shears off laterally gives incorrect result and if this occurs, the test should be repeated with another sample. If, in the repeat test also, the specimen shears, the slump should be measured and the fact that the specimen sheared, should be recorded.
Slump depends on many factors like properties of concrete ingredients – aggregates etc. Also temperature has its effect on slump value. So all these parameters should be kept in mind when deciding the ideal slump
Ques 2. How does a superplasticizer effect the slump of concrete?
Answer 2 Value of Slump can be increased by the addition of chemical admixtures like mid-range or high-range water reducing agents (super-plasticizers) without changing the water/cement ratio.
Ques 3. How much time one should take to raise the cone?
Answer 3 Once the cone is filled and topped off [ excessive concrete from top is cleared ] raise the cone within 5-10 seconds.
If you have a query, you can ask a question here.
Please Specifying me about concrete slump 1/3 mean our required Sepc is slump (180+- 1/3 of Specifiyed slump +-10mm)
What is the range of slump to be maintained for construction of bored piles by tremie concrete?
what shoild be the slump for m30 slab casting by pump at 60meter high kindly advise
what is the effect of slump in tempraure
If the same grade of concrete and in same condition is used for slump test then can we get different values and if then why.
i dont know how many reasons are there for your question..
but
according to my knowledge it happens because of human error.
like in proper mixing,
When is the right time for slump testing?